11SMn37 - Nr.1.0736

11SMn37 - Nr.1.0736Steel

High-Sulfur Free-Cutting Steel for Enhanced Machinability

Steel with the addition of sulfur only, in higher quantities than in 11SMn30; increased machinability at the expense of a slightly more accentuated fragility.

References and Comparable Standards

References and comparable standards for 11SMn37 steel
Region Standard Grade Werkstoff No.
Europe EN 10087: 1998
EN 10277-3: 2008
11SMn37 1.0736
Italy UNI 4838-80 CF9SMn36 -
Germany DIN 1651-88 9SMn36 1.0736
France NF A 35-561-92 S300 -
UK BS 970 pt.3-91 - -
USA ASTM A 29 - -
Europe

StandardEN 10087: 1998
EN 10277-3: 2008

Grade11SMn37

Werkstoff No.1.0736

Italy

StandardUNI 4838-80

GradeCF9SMn36

Werkstoff No.-

Germany

StandardDIN 1651-88

Grade9SMn36

Werkstoff No.1.0736

France

StandardNF A 35-561-92

GradeS300

Werkstoff No.-

UK

StandardBS 970 pt.3-91

Grade-

Werkstoff No.-

USA

StandardASTM A 29

Grade-

Werkstoff No.-

Chemical Composition (Cast Analysis) (%)

Chemical composition values for 11SMn37 steel
C / max Si / max Mn P / max S
0,14 0,05 1,00-1,50 0,11 0,34-0,40
Chemical composition values for 11SMn37 steel
Element Value (%)
Carbon 0,14
Silicon 0,05
Manganese 1,00-1,50
Phosphorus 0,11
Sulfur 0,34-0,40

Mechanical Properties - Bright Steel

Mechanical properties for 11SMn37 steel
Size (mm) as Rolled and/or as Rolled + Turned (+SH) Cold Drawn (+C)
Hardness

HB max
Tensile Strength

Rm (MPa)
Yield Strength

Rp0,2 (MPa) min
Tensile Strength

Rm (MPa)
Elongation

A5 (%) min
5≤d≤10 as Rolled and/or as Rolled + Turned (+SH)- as Rolled and/or as Rolled + Turned (+SH)- Cold Drawn (+C)440 Cold Drawn (+C)510-810 Cold Drawn (+C)6
10<d≤16 as Rolled and/or as Rolled + Turned (+SH)- as Rolled and/or as Rolled + Turned (+SH)- Cold Drawn (+C)410 Cold Drawn (+C)490-760 Cold Drawn (+C)7
16<d≤40 as Rolled and/or as Rolled + Turned (+SH)169 as Rolled and/or as Rolled + Turned (+SH)380-570 Cold Drawn (+C)375 Cold Drawn (+C)460-710 Cold Drawn (+C)8
40<d≤63 as Rolled and/or as Rolled + Turned (+SH)169 as Rolled and/or as Rolled + Turned (+SH)370-570 Cold Drawn (+C)305 Cold Drawn (+C)400-650 Cold Drawn (+C)9
63<d≤100 as Rolled and/or as Rolled + Turned (+SH)154 as Rolled and/or as Rolled + Turned (+SH)360-520 Cold Drawn (+C)245 Cold Drawn (+C)360-630 Cold Drawn (+C)9
Note: For size <5 mm the mechanical properties may be agreed at the time of enquiry and order.

Working Temperatures Recommended

Recommended working temperatures for 11SMn37 steel
Operation Temperature °C
Hot forgings deformation 950-1250 °C
Normalizing 870-910 °C
Soft annealing 650-700 °C
Published: 01 January 2025 | Last Updated: 26 May 2026
Products
Published: 01 January 2025 | Last Updated: 26 May 2026
Get a Quote Now
With over 30 years of experience and a wide product range, Bimeks Steel meets your private and commercial steel needs with the highest quality. Share your needs, product requests, or collaboration inquiries with us; our technical team will contact you as soon as possible to provide solution-oriented support.

E-mail

info@bimekscelik.com

Address copied!

Phone

(0216) 593 04 74

WhatsApp Call