Rodinox® Steel

Rodinox® Steel

What Is Rodinox Steel?

Rodinox® is a patented low-nickel austenitic stainless steel wire developed by Rodacciai. Its mechanical properties and corrosion resistance are similar to those of 1.4301 (AISI 304). It can replace AISI 304 in many applications. Its austenitic structure is achieved by balancing lower nickel with higher manganese, copper, and nitrogen contents. Rodacciai supplies Rodinox® as drawn wire for household goods, appliances, grills, racks, bicycle spokes, and clotheslines. Rodinox Plus® bars are also available with improved machinability.

Rodinox Steel: References and Comparable Standards

References and comparable standards for Rodinox steel
Region Standard Grade Werkstoff No.
Europe EN 10088-3: 2005 - -
Italy (UNI 6900:71) - -
Germany (DIN 1654-5: 89) - -
France (NF A 35-574-90) - -
UK (BS 3111 pt.2 -79) - -
USA AISI - -
Europe

StandardEN 10088-3: 2005

Grade-

Werkstoff No.-

Italy

Standard(UNI 6900:71)

Grade-

Werkstoff No.-

Germany

Standard(DIN 1654-5: 89)

Grade-

Werkstoff No.-

France

Standard(NF A 35-574-90)

Grade-

Werkstoff No.-

UK

Standard(BS 3111 pt.2 -79)

Grade-

Werkstoff No.-

USA

StandardAISI

Grade-

Werkstoff No.-

Rodinox Steel: Chemical Composition (Cast Analysis) (%)

Chemical composition values for Rodinox steel
  C Mn Si S* P Cr Ni Cu N
min - %5,00 - - - %16,00 %3,00 %1,00 %0,15
max %0,10 %9,00 %1,00 %0,015 %0,045 %19,00 %6,00 %4,00 %0,20
*For Rodinox Plus bars, S = 0,015 - 0,030
Chemical composition values for Rodinox steel
Carbon %0,10
Manganese %5,00-9,00
Silicon %1,00
Sulfur %0,015
Phosphorus %0,045
Chromium %16,00-19,00
Nickel %3,00-6,00
Copper %1,00-4,00
Nitrogen %0,15-0,20
*For Rodinox Plus bars, S = 0,015 - 0,030

Rodinox Steel: Mechanical Properties - Cold Drawn Wire And Coils (2H)*

Mechanical Properties - Cold Drawn Wire And Coils (2H)* for Rodinox steel
Tensile Strength Levels Tensile StrengthRm (MPa)
+C 600 600-800
+C 700 700-900
+C 800 800-1000
+C 900 900-1100
+C 1000 1000-1250
+C 1100 1100-1350
*For reference only.
Note: the desired tensile strength level
shall be evaluated depending on diameter required.

Rodinox Steel: Mechanical Properties - Cold Drawn Wire And Coils In The Solution Annealed Condition (2D)*

Mechanical Properties - Cold Drawn Wire And Coils In The Solution Annealed Condition (2D)* for Rodinox steel
Size(mm) Maximum ElongationA (%) max Tensile StrengthRm (MPa)
0,50≤d≤1,00 30 950
1,00≤d≤3,00 30 900
3,00≤d≤5,00 35 850
5,00≤d≤16,00 35 800
*For reference only.
Note: If skin passed, Rm might be increased by up to 50 MPa.

Rodinox Steel: Mechanical Properties - Bars, Wire And Coils For Cold Heading*

Mechanical Properties - Bars, Wire And Coils For Cold Heading* for Rodinox steel
Size
(mm)
As Treated
(+AT)
or
Peeled
(+AT+PE)
Cold Drawn
(+AT +C)
Cold Drawn + Solution annealed
(+AT +C +AT)
Cold Drawn + Solution annealed + Skin passed
(+AT +C +AT +LC)
Tensile StrengthRm (MPa) Reduction of AreaZ (%) min Tensile StrengthRm (MPa) Reduction of AreaZ (%) min Tensile StrengthRm (MPa) Reduction of AreaZ (%) min Tensile StrengthRm (MPa) Reduction of AreaZ (%) min
2≤d≤5 As Treated (+AT) or Peeled (+AT+PE)- As Treated (+AT) or Peeled (+AT+PE)- Cold Drawn (+AT +C)- Cold Drawn (+AT +C)- Cold Drawn + Solution annealed (+AT +C +AT)600 Cold Drawn + Solution annealed (+AT +C +AT)68 Cold Drawn + Solution annealed + Skin passed (+AT +C +AT +LC)650 Cold Drawn + Solution annealed + Skin passed (+AT +C +AT +LC)63
5<d≤10 As Treated (+AT) or Peeled (+AT+PE)590 As Treated (+AT) or Peeled (+AT+PE)68 Cold Drawn (+AT +C)740 Cold Drawn (+AT +C)- Cold Drawn + Solution annealed (+AT +C +AT)590 Cold Drawn + Solution annealed (+AT +C +AT)68 Cold Drawn + Solution annealed + Skin passed (+AT +C +AT +LC)640 Cold Drawn + Solution annealed + Skin passed (+AT +C +AT +LC)63
10<d≤25 As Treated (+AT) or Peeled (+AT+PE)590 As Treated (+AT) or Peeled (+AT+PE)68 Cold Drawn (+AT +C)740 Cold Drawn (+AT +C)- Cold Drawn + Solution annealed (+AT +C +AT)590 Cold Drawn + Solution annealed (+AT +C +AT)68 Cold Drawn + Solution annealed + Skin passed (+AT +C +AT +LC)- Cold Drawn + Solution annealed + Skin passed (+AT +C +AT +LC)-
25<d≤50 As Treated (+AT) or Peeled (+AT+PE)590 As Treated (+AT) or Peeled (+AT+PE)68 Cold Drawn (+AT +C)- Cold Drawn (+AT +C)- Cold Drawn + Solution annealed (+AT +C +AT)- Cold Drawn + Solution annealed (+AT +C +AT)- Cold Drawn + Solution annealed + Skin passed (+AT +C +AT +LC)- Cold Drawn + Solution annealed + Skin passed (+AT +C +AT +LC)-
* For reference only.

Rodinox Steel: Working Temperatures Recommended

Recommended working temperatures for Rodinox steel
Operation Temperature
Hot forgings deformation 900-1200 °C
Solution annealing (water, air) 1000-1100 °C
Published: 01 January 2025 | Last Updated: 21 November 2026

Other Stainless Steels Austenitic Products

Published: 01 January 2025 | Last Updated: 21 November 2026
Contact Us
With over 37 years of experience and a wide product range, Bimeks Çelik meets your steel needs. Please share your material and technical support inquiries with us. Our expert team will get in touch with you shortly to provide support.

E-mail

info@bimekscelik.com